Introduction to cast iron welding rods and welding precautions

Jan 08, 2024 Leave a message

Due to its high carbon content, uneven structure, and low plasticity, cast iron is considered a material with poor weldability. During the welding process, defects such as white spots, cracks, and pores are prone to occur. Therefore, cast iron welding repair also requires a high level of technical proficiency from the welder. Cast iron welding repair can be divided into two types: preheating welding and cold welding.

To ensure welding effectiveness, it is recommended to use the following welding measures for reference and selection when repairing castings of different materials and defects.
EZC type gray cast iron welding rod
EZC type steel core strongly graphitized coated cast iron welding rod, can be used for both AC and DC. Adding an appropriate amount of graphitic elements to the coating of steel core cast iron welding rods can transform the weld into gray cast iron when slowly cooled. If the cooling speed is fast, white spots will be produced and it is not easy to process. The cooling rate has a significant impact on the machinability and weld microstructure, as the operating process is different from that of general cold welding electrodes. This electrode requires continuous welding and post welding insulation to slow down the weld. The microstructure, properties, and color of gray cast iron welding joints are basically similar to the base metal, but due to poor plasticity, welding stress cannot be relaxed, resulting in poor thermal stress cracking performance. Defects in small thin-walled parts with lower stiffness can be welded without preheating, but generally should be preheated to around 400 before welding, and slowly cooled after welding to prevent cracks and white spots.

 

1

 

EZNi type pure nickel cast iron welding rod
EZNi type is a pure nickel core strongly graphitized coated cast iron welding rod, which can be used for both AC and DC, and can be used for all position welding. When welding, the welded part may not be preheated. It is a type of welding rod with good comprehensive properties such as crack resistance, machinability, operating technology, and mechanical properties in cast iron cold welding. It is widely used for repairing welding of thin cast iron parts and machining surfaces.
EZNiFe type pure nickel cast iron welding rod
EZNiFe type is a cast iron welding rod with pure nickel core and strong graphite coating, which can be used for both AC and DC, and can be used for all position welding. When welding, the welded part does not need to be preheated, and has the characteristics of high strength, good plasticity, excellent cracking resistance, and good fusion with the base material. Can be used for repairing welding of important gray cast iron and ductile iron.
EZNiCu type nickel copper cast iron welding rod EZNiCu type is a cast iron welding rod with a nickel copper alloy welding core and strong graphitic coating. It can be used for both AC and DC, and can be used for all position welding. The process performance and cutting performance are similar to those of welding rods, but due to the high shrinkage rate and low tensile strength of the weld metal, it is not suitable for repairing welding of castings with high stiffness. It can be preheated to around 300 at room temperature or low temperature for welding. Used for repairing welding of gray castings with low strength requirements and good plasticity requirements.